Home > News > Content

API Black Seamless Steel Pipe/Tube, API 5L ERW Pipe/Tube, ASTM A106 Line Pipe/Tube

Dec 23, 2016
Basic Info
  • Model NO.: API black seamless steel pipe

  • Technique: Hot Rolled

  • Surface Treatment: Black

  • Section Shape: Round

  • Trademark: luzheng

  • Origin: Shandong, China

  • Type: Seamless

  • Material: Carbon Steel

  • Usage: Pipeline Transport, Oil/Gas Drilling

  • API5l: B,X42,X52,X60

  • Specification: OD from 1/2inch to 42inch

  • HS Code: 7304192000

Product Description
Seamless  Steel Line Pipe in API 5L PSL1/PSL2
Sch20,Sch30,,Sch40,STD,Sch60,Sch80,Sch100,Sch120,Sch140

It is used for conveying gas,water,and petroleum of both the oil and natural gas industries.
Grade:GR.B.X42,X46,X52,X56,X60,X70
For any other seamless tube,we can aslo supply DIN,EN ,ASTM/ASME.GOST,GB.

TYPEgradeTensile strength
(Mpa)
Yield strength
(Mpa)
Elongation
API 5L PSL1B≥415≥245As per API 5L
API 5L PSL1X42≥415≥290As per API 5L
API 5L PSL1X52≥460≥360As per API 5L
API 5L PSL1X56≥490≥390As per API 5L
API 5L PSL1X60≥520≥415As per API 5L
API 5L PSL1X65≥535≥450As per API 5L
API 5L PSL1X70≥565≥483As per API 5

Mechanical Properties

TYPEgradeTensile strength
(Mpa)
Yield strength
(Mpa)
Elongation
API 5L PSL1B≥415≥245As per API 5L
API 5L PSL1X42≥415≥290As per API 5L
API 5L PSL1X52≥460≥360As per API 5L
API 5L PSL1X56≥490≥390As per API 5L
API 5L PSL1X60≥520≥415As per API 5L
API 5L PSL1X65≥535≥450As per API 5L
API 5L PSL1X70≥565≥483As per API 5L
 